{"_buckets": {"deposit": "78abadc8-1857-4980-81bb-0181e9851448"}, "_deposit": {"id": "12421", "owners": [], "pid": {"revision_id": 0, "type": "depid", "value": "12421"}, "status": "published"}, "_oai": {"id": "oai:soar-ir.repo.nii.ac.jp:00012421", "sets": ["1222"]}, "author_link": ["37852", "37853"], "item_1628147817048": {"attribute_name": "出版タイプ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_6_alternative_title_1": {"attribute_name": "その他(別言語等)のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "Detection of a tiny metal wire using induction gradiometer"}]}, "item_6_biblio_info_6": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2009-06-10", "bibliographicIssueDateType": "Issued"}, "bibliographicIssueNumber": "2", "bibliographicPageEnd": "359", "bibliographicPageStart": "354", "bibliographicVolumeNumber": "17", "bibliographic_titles": [{"bibliographic_title": "日本AEM学会誌"}]}]}, "item_6_description_20": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "A magnetic contamination detection system based on high sensitive induction gradiometer is presented. This system is free from heavy cooling system, and the magnetic sensor consists of coil and simple electronics only. This paper considers the detection limit of two kinds of wire, SUS304 and Fe. It is found that the detection limit and profile of output signal are differs from the wire material. When the length of wire is 10mm, our system can detect a SUS304 wire having 0.2mm diameter, and an Fe wire having 0.1mm diameter.", "subitem_description_type": "Abstract"}]}, "item_6_description_30": {"attribute_name": "資源タイプ(コンテンツの種類)", "attribute_value_mlt": [{"subitem_description": "Article", "subitem_description_type": "Other"}]}, "item_6_description_5": {"attribute_name": "引用", "attribute_value_mlt": [{"subitem_description": "日本AEM学会誌. 17(2):354-359 (2009)", "subitem_description_type": "Other"}]}, "item_6_link_3": {"attribute_name": "信州大学研究者総覧へのリンク", "attribute_value_mlt": [{"subitem_link_text": "田代, 晋久", "subitem_link_url": "http://soar-rd.shinshu-u.ac.jp/profile/ja.gVSVjefp.html"}, {"subitem_link_text": "脇若, 弘之", "subitem_link_url": "http://soar-rd.shinshu-u.ac.jp/profile/ja.OFcFZVkh.html"}]}, "item_6_publisher_4": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "日本AEM学会"}]}, "item_6_relation_51": {"attribute_name": "異版である", "attribute_value_mlt": [{"subitem_relation_type": "isVersionOf", "subitem_relation_type_id": {"subitem_relation_type_id_text": "http://ci.nii.ac.jp/naid/110007333990", "subitem_relation_type_select": "URI"}}]}, "item_6_rights_62": {"attribute_name": "権利", "attribute_value_mlt": [{"subitem_rights": "Copyright© 2009 日本AEM学会"}, {"subitem_rights": "本文データは学協会の許諾に基づきCiNiiから複製したものである"}]}, "item_6_select_64": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_select_item": "publisher"}]}, "item_6_source_id_35": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0919-4452", "subitem_source_identifier_type": "ISSN"}]}, "item_6_source_id_39": {"attribute_name": "NII ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0919-4452", "subitem_source_identifier_type": "ISSN"}]}, "item_6_source_id_40": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_source_identifier": "AN10457520", "subitem_source_identifier_type": "NCID"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "田代, 晋久"}], "nameIdentifiers": [{"nameIdentifier": "37852", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "脇若, 弘之"}], "nameIdentifiers": [{"nameIdentifier": "37853", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2015-09-28"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "Detection_tiny_metal_wire.pdf", "filesize": [{"value": "1.4 MB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_note", "mimetype": "application/pdf", "size": 1400000.0, "url": {"label": "Detection_tiny_metal_wire.pdf", "url": "https://soar-ir.repo.nii.ac.jp/record/12421/files/Detection_tiny_metal_wire.pdf"}, "version_id": "c8e7392a-77d9-4bf9-aae3-e4d5758ab0b2"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "nondestructive evaluation", "subitem_subject_scheme": "Other"}, {"subitem_subject": "magnetic contamination detection system", "subitem_subject_scheme": "Other"}, {"subitem_subject": "induction gradiometer", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "インダクション磁気センサを用いた微小金属片検出", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "インダクション磁気センサを用いた微小金属片検出", "subitem_title_language": "ja"}]}, "item_type_id": "6", "owner": "1", "path": ["1222"], "permalink_uri": "http://hdl.handle.net/10091/15909", "pubdate": {"attribute_name": "PubDate", "attribute_value": "2012-07-23"}, "publish_date": "2012-07-23", "publish_status": "0", "recid": "12421", "relation": {}, "relation_version_is_last": true, "title": ["インダクション磁気センサを用いた微小金属片検出"], "weko_shared_id": -1}
インダクション磁気センサを用いた微小金属片検出
http://hdl.handle.net/10091/15909
http://hdl.handle.net/10091/1590946d4f8a0-92a0-4292-bff5-31de08e3a32c
名前 / ファイル | ライセンス | アクション |
---|---|---|
![]() |
|
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2012-07-23 | |||||
タイトル | ||||||
言語 | ja | |||||
タイトル | インダクション磁気センサを用いた微小金属片検出 | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | nondestructive evaluation | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | magnetic contamination detection system | |||||
キーワード | ||||||
主題Scheme | Other | |||||
主題 | induction gradiometer | |||||
資源タイプ | ||||||
資源 | http://purl.org/coar/resource_type/c_6501 | |||||
タイプ | journal article | |||||
その他(別言語等)のタイトル | ||||||
その他のタイトル | Detection of a tiny metal wire using induction gradiometer | |||||
著者 |
田代, 晋久
× 田代, 晋久× 脇若, 弘之 |
|||||
信州大学研究者総覧へのリンク | ||||||
氏名 | 田代, 晋久 | |||||
URL | http://soar-rd.shinshu-u.ac.jp/profile/ja.gVSVjefp.html | |||||
信州大学研究者総覧へのリンク | ||||||
氏名 | 脇若, 弘之 | |||||
URL | http://soar-rd.shinshu-u.ac.jp/profile/ja.OFcFZVkh.html | |||||
出版者 | ||||||
出版者 | 日本AEM学会 | |||||
引用 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 日本AEM学会誌. 17(2):354-359 (2009) | |||||
書誌情報 |
日本AEM学会誌 巻 17, 号 2, p. 354-359, 発行日 2009-06-10 |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | A magnetic contamination detection system based on high sensitive induction gradiometer is presented. This system is free from heavy cooling system, and the magnetic sensor consists of coil and simple electronics only. This paper considers the detection limit of two kinds of wire, SUS304 and Fe. It is found that the detection limit and profile of output signal are differs from the wire material. When the length of wire is 10mm, our system can detect a SUS304 wire having 0.2mm diameter, and an Fe wire having 0.1mm diameter. | |||||
資源タイプ(コンテンツの種類) | ||||||
内容記述タイプ | Other | |||||
内容記述 | Article | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 0919-4452 | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN10457520 | |||||
異版である | ||||||
関連タイプ | isVersionOf | |||||
識別子タイプ | URI | |||||
関連識別子 | http://ci.nii.ac.jp/naid/110007333990 | |||||
権利 | ||||||
権利情報 | Copyright© 2009 日本AEM学会 | |||||
権利 | ||||||
権利情報 | 本文データは学協会の許諾に基づきCiNiiから複製したものである | |||||
出版タイプ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 |