WEKO3
アイテム
{"_buckets": {"deposit": "5f335630-1df5-4071-b8ff-ce895e455c45"}, "_deposit": {"id": "14576", "owners": [], "pid": {"revision_id": 0, "type": "depid", "value": "14576"}, "status": "published"}, "_oai": {"id": "oai:soar-ir.repo.nii.ac.jp:00014576", "sets": ["1462"]}, "author_link": ["43905", "43906"], "item_11_alternative_title_1": {"attribute_name": "その他(別言語等)のタイトル", "attribute_value_mlt": [{"subitem_alternative_title": "シルクフィブロイン - セルロース複合再生繊維の実用性能"}]}, "item_11_biblio_info_6": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2004-03-31", "bibliographicIssueDateType": "Issued"}, "bibliographicPageEnd": "44", "bibliographicPageStart": "44", "bibliographicVolumeNumber": "10", "bibliographic_titles": [{"bibliographic_title": "先進ファイバー工学研究教育拠点研究成果報告書"}]}]}, "item_11_description_20": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "We tried to prepare micro silk powder by grinding silk filaments. Such micro-silk powder should be fine enough to be included in the viscose-rayon fibers, which are formed by extruding a viscous polymer solution from very small mouthpieces. First, a treatment of roughly ground silk powder by hot alkaline water was tried expecting that the alkali dissolves the silk particles at their edges to make sphere-shaped micro powders. Although this method was not successful, resulting silk particles showed a novel flake-shaped appearance on which we have had some expectations to utilize for purposes other than fiber materials. Gamma ray irradiation on silk filaments was quite effective in weakening the mechanical strength of the fibers. Silk filaments exposed to 2000 Gy gamma ray were easily ground into fine particles around 1 /1m in diameter only by grinding by ordinal ball-mills.", "subitem_description_type": "Abstract"}]}, "item_11_description_30": {"attribute_name": "資源タイプ(コンテンツの種類)", "attribute_value_mlt": [{"subitem_description": "Article", "subitem_description_type": "Other"}]}, "item_11_description_5": {"attribute_name": "引用", "attribute_value_mlt": [{"subitem_description": "先進ファイバー工学研究教育拠点研究成果報告書 10: 44-44(2004)", "subitem_description_type": "Other"}]}, "item_11_link_3": {"attribute_name": "信州大学研究者総覧へのリンク", "attribute_value_mlt": [{"subitem_link_text": "木口, 憲爾", "subitem_link_url": "http://soar-rd.shinshu-u.ac.jp/profile/ja.uFDajekV.html"}]}, "item_11_publisher_4": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "信州大学繊維学部"}]}, "item_11_select_64": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_select_item": "publisher"}]}, "item_11_source_id_40": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_source_identifier": "AA1200368X", "subitem_source_identifier_type": "NCID"}]}, "item_11_text_66": {"attribute_name": "sortkey", "attribute_value_mlt": [{"subitem_text_value": "014"}]}, "item_1627890728808": {"attribute_name": "出版タイプ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "金勝, 康介"}], "nameIdentifiers": [{"nameIdentifier": "43905", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "木口, 憲爾"}], "nameIdentifiers": [{"nameIdentifier": "43906", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2015-09-28"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "AFSTT10-202.pdf", "filesize": [{"value": "478.2 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_note", "mimetype": "application/pdf", "size": 478200.0, "url": {"label": "AFSTT10-202.pdf", "url": "https://soar-ir.repo.nii.ac.jp/record/14576/files/AFSTT10-202.pdf"}, "version_id": "5e592bd9-ee07-4825-b212-ff8380205170"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "research report", "resourceuri": "http://purl.org/coar/resource_type/c_18ws"}]}, "item_title": "15-2-2 :マイクロシルクパウダーの作成条件", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "15-2-2 :マイクロシルクパウダーの作成条件", "subitem_title_language": "ja"}]}, "item_type_id": "11", "owner": "1", "path": ["1462"], "permalink_uri": "http://hdl.handle.net/10091/13583", "pubdate": {"attribute_name": "PubDate", "attribute_value": "2012-02-23"}, "publish_date": "2012-02-23", "publish_status": "0", "recid": "14576", "relation": {}, "relation_version_is_last": true, "title": ["15-2-2 :マイクロシルクパウダーの作成条件"], "weko_shared_id": -1}
15-2-2 :マイクロシルクパウダーの作成条件
http://hdl.handle.net/10091/13583
http://hdl.handle.net/10091/1358346597066-abbb-4ac8-a00f-693ab3d58914
名前 / ファイル | ライセンス | アクション |
---|---|---|
![]() |
|
Item type | 研究報告書 / Research Paper(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2012-02-23 | |||||
タイトル | ||||||
言語 | ja | |||||
タイトル | 15-2-2 :マイクロシルクパウダーの作成条件 | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源 | http://purl.org/coar/resource_type/c_18ws | |||||
タイプ | research report | |||||
その他(別言語等)のタイトル | ||||||
その他のタイトル | シルクフィブロイン - セルロース複合再生繊維の実用性能 | |||||
著者 |
金勝, 康介
× 金勝, 康介× 木口, 憲爾 |
|||||
信州大学研究者総覧へのリンク | ||||||
氏名 | 木口, 憲爾 | |||||
URL | http://soar-rd.shinshu-u.ac.jp/profile/ja.uFDajekV.html | |||||
出版者 | ||||||
出版者 | 信州大学繊維学部 | |||||
引用 | ||||||
内容記述タイプ | Other | |||||
内容記述 | 先進ファイバー工学研究教育拠点研究成果報告書 10: 44-44(2004) | |||||
書誌情報 |
先進ファイバー工学研究教育拠点研究成果報告書 巻 10, p. 44-44, 発行日 2004-03-31 |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | We tried to prepare micro silk powder by grinding silk filaments. Such micro-silk powder should be fine enough to be included in the viscose-rayon fibers, which are formed by extruding a viscous polymer solution from very small mouthpieces. First, a treatment of roughly ground silk powder by hot alkaline water was tried expecting that the alkali dissolves the silk particles at their edges to make sphere-shaped micro powders. Although this method was not successful, resulting silk particles showed a novel flake-shaped appearance on which we have had some expectations to utilize for purposes other than fiber materials. Gamma ray irradiation on silk filaments was quite effective in weakening the mechanical strength of the fibers. Silk filaments exposed to 2000 Gy gamma ray were easily ground into fine particles around 1 /1m in diameter only by grinding by ordinal ball-mills. | |||||
資源タイプ(コンテンツの種類) | ||||||
内容記述タイプ | Other | |||||
内容記述 | Article | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AA1200368X | |||||
出版タイプ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 |